What We Currently Know

  • Approximately 20 reported cases of freeze-related deterioration installations 2020/2022
  • Reported issues include cracking, spalling and surface delamination following freeze–thaw cycles
  • Independent laboratory testing has been conducted on sample tiles (summary available)

Reports originate from multiple UK regions